MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Green Dot Terratek® WC200180 (Preliminary) Nylon, Wood Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Product Description: Terratek® WC200180 is a proprietary blend of wood fiber and nylon for injection molding applications.

Information provided by Green Dot Bioplastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/in
Melt Flow 3.2 g/10 min3.2 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 72.547 MPa10522 psiASTM D638
Elongation at Break 2.08 %2.08 %
Tensile Modulus 4.7790 GPa693.14 ksiASTM D638
Flexural Strength 124.35 MPa18035 psiASTM D790
Flexural Modulus 3.99690 GPa579.702 ksiASTM D790
Izod Impact, Notched 0.358 J/cm0.670 ft-lb/inASTM D256
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 177 - 182 °C350 - 360 °F
Middle Barrel Temperature 177 - 182 °C350 - 360 °F
Front Barrel Temperature 182 - 191 °C360 - 375 °F
Nozzle Temperature 182 - 191 °C360 - 375 °F
Melt Temperature <= 204 °C<= 400 °F
Mold Temperature 15.6 - 76.7 °C60.0 - 170 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGREEND5037 / 312308

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.