MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polymer Resources NY66-IM2 Impact Modified Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Nylon 66, Superior Impact Modified, Lubricated

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).

Information provided by Polymer Resources Corporation.

Key Words: UL E113219
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccASTM D792
Linear Mold Shrinkage 0.017 - 0.020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7300 psiASTM D638
Tensile Strength, Yield 7500 psiASTM D638
Flexural Strength 9000 psiASTM D790
Flexural Modulus 245 ksiASTM D790
Izod Impact, Notched 16.0 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Gardner Impact 320 in-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 415 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 155 °FASTM D648
UL RTI, Electrical 149 °F
@Thickness 1.50 mm
UL 746
 149 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 149 °F
@Thickness 1.50 mm
UL 746
 149 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 149 °F
@Thickness 1.50 mm
UL 746
 149 °F
@Thickness 3.00 mm
UL 746
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 510 - 530 °F
Middle Barrel Temperature 520 - 540 °F
Front Barrel Temperature 530 - 550 °F
Melt Temperature 530 - 560 °F
Mold Temperature 150 - 200 °F
Drying Temperature 165 - 185 °F
Dry Time 3.00 - 4.00 hour
Vent Depth 0.000300 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 203 H Impact-Modified Nylon 6/6 (PA), Glass Fiber
RTP Company RTP 205 H Impact-Modified Nylon 6/6 (PA), Glass Fiber
RTP Company RTP 207 H Impact-Modified Nylon 6/6 (PA), Glass Fiber
Omni Plastics OmniLon™ 6 PA6 GR30 IM6 Glass Reinforced/Impact Modified Nylon
Nylene® 4214-33 (HS) 33% Glass Fiber Reinforced Impact Modified Nylon 6

PPOLYQ049 / 160564

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.