DANRESIN® W 44 is an aqueous, anionic, tacky adhesive resin emulsion, which is added as a tackifier of polyurethane- and acrylate dispersion adhesives. The product has already been proved for other dispersions and the modifying characteristics are excellent. DANRESIN® W 44 is a protective colloid free resin emulsion, which is added to aqueous adhesive systems to prolong the „ open time “, the contact adhesion, the pressure sensitivity by one-side adhesives and to improve the reactivating characteristics of adhesives. Application: DANRESIN® W 44 is used as a tackifier modified resin emulsion during the production of aqueous contact adhesives and aqueous one-way adhesives on the basis of acrylate-, NBR-, SBR-, PUR-, PCP-, VA- and EVA-polymer-dispersions. Additives of DANRESIN® W 44 are able to improve the “open time” with polyurethane adhesives which are adhered after heat reactivation and drying. ( HOT-TACK-TIME-LIFE ). Information provided by Danquinsa GMBH |