MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC Ultem 1110R PEI (Europe-Africa-Middle East)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.

This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.36 g/ccASTM D 792
Density 1.36 g/ccISO 1183
Moisture Absorption at Equilibrium 0.65 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.2 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cmon tensile bar; SABIC Method
 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 16 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D 1238
 21 g/10 min
@Load 5.00 kg,
Temperature 360 °C
[cm^3/10 min] Melt Volume Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPa5 mm/min; ISO 527
 85.0 MPaType I, 5 mm/min; ASTM D 638
Tensile Strength, Yield 110 MPaType I, 5 mm/min; ASTM D 638
 110 MPa5 mm/min; ISO 527
Elongation at Break 60 %5 mm/min; ISO 527
 70 %Type I, 5 mm/min; ASTM D 638
Elongation at Yield 6.0 %5 mm/min; ISO 527
 7.0 %Type I, 5 mm/min; ASTM D 638
Tensile Modulus 3500 MPa1 mm/min; ISO 527
 3720 MPa5 mm/min; ASTM D 638
Flexural Yield Strength 140 MPa2 mm/min; ISO 178
 165 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 3300 MPa2 mm/min; ISO 178
 3720 MPa1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 56.0 J/m
@Temperature 23.0 °C
ASTM D 256
 1920 J/m
@Thickness 3.20 mm
reverse notched; ASTM D 256
Izod Impact, Unnotched 21.0 J/cm
@Temperature 23.0 °C
ASTM D 4812
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Gardner Impact 23.0 J
@Temperature 23.0 °C
ASTM D 3029
Instrumented Impact Total Energy 28.0 J
@Temperature 23.0 °C
ASTM D 3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 3.5
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 17.2 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor 0.0016
@Frequency 50.0 - 60.0 Hz
IEC 60250
Comparative Tracking Index >= 125 VIEC 60112
 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 55.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E 831
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 55.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E 831
Thermal Conductivity 0.260 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 200 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 207 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
 210 °C
@Thickness 6.40 mm
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 185 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 197 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
 199 °C
@Thickness 6.40 mm
unannealed; ASTM D 648
Vicat Softening Point 200 °CRate B/50; ISO 306
 205 °CRate B/120; ISO 306
 210 °CRate A/50; ISO 306
 219 °CRate B/50; ASTM D 1525
Glass Transition Temp, Tg 217 °C
 
Descriptive Properties
Ball Pressure Test, 125°C +/- 2°CPassesIEC 60695-10-2

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SABIC Ultem 1110R PEI

PSABIC6086 / 119974

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.