LNP LUBRICOMP RFP36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. This product is also known as LUBRICOMP* RFL-4536.Information provided by SABIC Innovative Plastics for Asia Pacific. |