MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BCC Products BX-31 Urethane Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Applications: BX-31 is used to make molds of masters that contain moderate undercuts. BX- 31’s physical properties make it ideal for making detailed concrete molds, patterns and formliners.

Characteristics: BX-31 is a two-part polyurethane molding system. BX-31 is mixed 100iso:97curative by weight (or 1 Pt-A Iso to 1 Pt-B Curative by volume) and cures at room temperature. BX-31 cures to a low hardness, Shore A 31? 2, light yellow rubber. Ultimate properties are obtained after 3-4 days of room temperature cure. Cure can be accelerated with heat (130-150°F for 12-16 hours) but a slightly harder polymer (34 +/- 2 Shore A) and slight shrinkage will be obtained.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.23 lb/galCurative (Part B)
 8.46 lb/galIso (Part A)
Viscosity 325 - 375 cPCurative (Part B)
 900 - 1100 cPIso (Part A)
Storage Temperature 16.0 - 32.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 29 - 33
Tensile Strength >= 300 psiASTM D412
Elongation at Break >= 1000 %ASTM D412
Tear Strength 16.0 - 24.0 plisplit; ASTM D470
 >= 70.0 pliDie C; ASTM D624-C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 minMix Time
 24.0 hourDemold Time
 72.0 hourComplete Cure Time
Pot Life 20.0 - 25.0 min
Gel Time 25.0 - 35.0 min
Shelf Life 6.00 MonthIso (Part A)
 6.00 MonthCurative (Part B)
 6.00 Month
 
Descriptive Properties
ColorClear light yellow to amberIso (Part A)
 Opaque light yellowCurative (Part B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBCC113 / 250978

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.