Applications: 2,9-Dimethyl-4,7-diphenyl-1,10-phenanthroline, also known as Bathocuproine (BCP), is a wide-band-gap material and has a high electron affinity. When it is embedded into organic electronic devices, bathocuproine acts as an exciton-blocking barrier which prohibits exciton diffusion process towards the Al electrode otherwise being quenched. One of the most commonly used buffer layer between acceptor and cathode layers is bathocuproine. The introduction of the buffer layer can greatly improve the PCE of polymer organic solar cells. BCP is one of the most popular hole-blocking layer materials that is used in organic electronics, including perovskite solar cells.
It was demonstrated that a BCP buffer layer reduces nonradiative recombination of excitons at the C60 -Al interface. Its most important function is to establish an Ohmic contact between the C60 film and the Al electrode in photovoltaic devices.Molecular Formula: C26H20N2 IUPAC Name: 2,9-dimethyl-4,7-diphenyl-1,10-phenanthroline Synonyms: SBB008863; 2, 9-Dimethyl-4, 7-diphenyl-1, 10-phenanthroline; KS-00000IQG; 92127-EP2272828A1; VZ23039; 2,9-dimethyl-4,7-diphenyl-1,10-phenanthroline/Bathocuproine; EINECS 225-240-5; BCP11188; AM62655; NSC 89195; SMILES: CC1=NC2=C(C=CC3=C2N=C(C=C3C4=CC=CC=C4)C)C(=C1)C5=CC=CC=C5; InChI=1S/C26H20N2/c1-17-15-23(19-9-5-3-6-10-19)21-13-14-22-24(20-11-7-4-8-12-20)16-18(2)28-26(22)25(21)27-17/h3-16H,1-2H3;; InChiKey = STTGYIUESPWXOW-UHFFFAOYSA-N; Alfa Chemistry Materials product group: Ligands for Functional Metal Complexes; Organic Light-Emitting Diode (OLED) Materials; Organic Solar Cell (OPV) Materials; Perovskite Solar Cell (PSC) Materials; Sublimed Materials Manufacturer data sheet |
Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |