MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Zeon Specialty Materials Zeonex® 490K Cyclo Olefin Optical Grade Polymer
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: Pencil hardness (JIS K5401) is 'H'. Major applications of Zeonex® 490K include optical films.

General Zeonex® Information: Specific grades of Zeonex® are available for different applications. Zeonex® features include chemical resistance to acids and bases, low impurity content, and easy processing through injection molding, blow molding, and film extrusion. Specific grades are used in camera lenses, prisms, and VTR lenses; CD pickup lenses, LBP FΘ lenses, and polygon mirrors; films; and other uses in the electric, electronic, medical treatment, and optronics fields.

Information provided by Zeon Chemicals L.P.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccASTM D792
Water Absorption <= 0.010 %ASTM D570
Moisture Vapor Transmission 0.230 cc-mm/m²-24hr-atmg-mm/m²-24 hr; (100µm) JIS Z 0208
Melt Flow 16 g/10 min280°C/2.16 kg; JIS K 6719
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 61.0 MPaASTM D638
Elongation at Break 90 %ASTM D638
Tensile Modulus 2.30 GPaASTM D638
Flexural Yield Strength 94.0 MPaASTM D790
Flexural Modulus 2.10 GPaASTM D790
Izod Impact, Notched 0.230 J/cm
@Thickness 3.20 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.27
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 40.0 kV/mm
@Thickness 1.00 mm
short time; ASTM D149
Dissipation Factor 0.00020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 124 °CUnannealed; ASTM D648
Glass Transition Temp, Tg 140 °CDSC
Flammability, UL94 HB
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.525ASTM D542
Transmission, Visible 92 %
@Thickness 3.00 mm
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZEON7 / 72958

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.