Description: ElastiSeal® 6098 is a non-flowing sealant designed to waterproof and prevent corrosion in spot weld assem¬blies. This sealant permits welding with conventional spot welders, it prevents moisture and oxygen from en¬tering the joint, and provides corrosion protection to the area that cannot be coated with primer. The sealant dis¬appears from the area of the weld but retains a tight seal around the weld spot, weld strengths are unchanged by the use of ElastiSeal® 6098. Features: - Prevents corrosion in a variety of steel spot welds – Including stainless steel
- Does not affect weld strength
- Weldable with conventional spot welders
- Remains permanently flexible and elastic
- Will not stain or bleed through most primers and paints
- Not affected by paint bake temperatures up to 90°C (195°F)
Application: ElastiSeal® 6098 can be applied as a bead or spread as a paste. Welds may be made through the sealer from 10 minutes to 72 hours after application. (“Spitting” may occur if welding is performed before solvent escapes.) This sealer is unaffected by conventional industrial paint bakes. Excess material may be wiped off with mineral spirits; use mineral spirits to clean tools and equipment.Information provided by H.B. Fuller Company |