MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Phillips 66 Kendall® Hyken® Glacial Blu Hydraulic Fluid ISO Grade 15
Categories: Fluid; Lubricant

Material Notes: Kendall® Hyken Glacial Blu Hydraulic Fluid is a high-quality, low-viscosity antiwear hydraulic oil specially developed for use in industrial and mobile equipment operating at extremely low temperatures. It has a very high viscosity index and a low pour point for use in arctic conditions. Hyken Glacial Blu Hydraulic Fluid is formulated to provide outstanding low-temperature properties, excellent wear protection for hydraulic pumps and motors, resistance to deposit formation, and protection against rust and corrosion. It has excellent water-separating properties to minimize the formation of emulsions, and is resistant to excessive foam buildup that can cause poor or sluggish hydraulic system response. Hyken Glacial Blu Hydraulic Fluid may be used in land-based hydraulic systems where the equipment manufacturer specifies a MIL-H-5606 fluid. It is not recommended for aircraft use.

Applications:

  • Industrial and mobile equipment operating in cold climates
  • Bucket trucks (cherry pickers) used for servicing electrical power lines or for tree-trimming
  • Surface mining equipment
Features/Benefits:
  • Outstanding low-temperature properties
  • Very high viscosity index for use in arctic conditions
  • Good wear protection for hydraulic pumps and motors
  • Resists deposit formation and viscosity increase due to oxidation
  • Protects against rust and corrosion
  • Excellent water-separating properties
  • Good foam resistance
  • High dielectric strength for use in electrical service bucket trucks

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.855 g/cc
Density 7.12 lb/gal
Brookfield Viscosity 2840 cP
@Temperature -40.0 °C
Viscosity Measurement 233Index
Saybolt Viscosity at 100°F 80.8 SUS
Saybolt Viscosity at 210°F 41 SUS
Kinematic Viscosity at 40°C (104°F) 14.9 cSt
Kinematic Viscosity at 100°C (212°F) 4.4 cSt
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.50[mg KOH/g]; ASTM D974
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 35.0 kV/mmASTM D877
 
Thermal PropertiesOriginal ValueComments
Pour Point -60.0 °C
Flash Point 171 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn 0.042 %
 
Descriptive Properties
ColorBlue
Demulsibility10 minutes to passASTM D1401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5321 / 198574

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.