MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Huber HN 434 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: HN-434 is a halogen–free, fine particle size ATH product that provides low cost flame retardant and smoke suppression in a variety of applications. The particle size distribution is specifically designed for low viscosity, high filler loading levels, and excellent processing characteristics, up to 200°C.

Applications: A closely controlled top size with a large superfine fraction yields rapid dispersion in resin. Excellent mold flow and wetout characteristics result in superior surface profile with minimal porosity, even pigmentation and excellent filler and reinforcement distribution throughout the molded part. HN-434 is recommended for spray-up or hand-lay up FRP applications, filament winding, panel production, resin injection, foam materials, cast polymer and epoxy parts, coatings, adhesives, latex, vinyl and urethane compounds.

Physical Form: White powder

Morphology: Hexagonal Platelets

Generic Type: Aluminum trihydrate

CAS No.: 21645-51-2

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.42 g/cc2.42 g/cc
Bulk Density 1.10 g/cc0.0397 lb/in³packed
Brightness 94 %94 %Ry
Oil Absorption >= 22 %>= 22 %22 ml/100gm
Particle Size <= 1.0 µm<= 1.0 µmScreen Analysis: 8.6 percent
 9.5 µm9.5 µmMedian Particle Diameter
 <= 10 µm<= 10 µmScreen Analysis: 51.3 percent
 <= 45 µm<= 45 µmScreen Analysis: 99 percent
Specific Surface Area 3.0 m²/g3.0 m²/gBET
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 3.03.0
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 7700 ohm-cm>= 7700 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 <= 0.020 %<= 0.020 %
Free Water 0.35 %
@Temperature 105 °C
0.35 %
@Temperature 221 °F
TGA
Loss on Ignition(%) 34.5 %
@Temperature 550 °C
34.5 %
@Temperature 1020 °F
Na2O 0.030 %0.030 %soluble
 0.20 %0.20 %total
SiO2 <= 0.040 %<= 0.040 %
 
Descriptive Properties
Al(OH)3 (%)99.6
CIELAB, L*98
ColorWhite powder
FunctionalitySmoke Suppression
Market/Application: Building & ConstructionPaints & Coatings
Market/Application: ThermosetsSMC/BMC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER703 / 300809

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.