Very low viscosity for rapid saturation of fiberglass, Kevlar® and carbon fiber laminate with resin infusion and VARTM processes. Fast speed hardener provides up to 40 minutes of pot life at 72°F (22°C). Optimized for hand wet out and machine impregnation in contact molding, vacuum bagging and filament winding applications. Room temperature cure properties suitable for many composite components and structures. Tg as high as 151°F (66°C) with proper post cure providing excellent temperature stability and great part cosmetics. Cost effective, high performance epoxy formulation for synthetic composite manufacturing. Quality-control tinting is available at no extra charge; simply add "QC" after the product code on your order.Information provided by Gougeon Brothers, Inc. |