MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Epoxies, Etc 20-3401 Medical, Optical and Semiconductor Grade Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 20-3401 is a two component clear epoxy resin system. It provides excellent optical transmission properties along with outstanding adhesion and electrical insulation. 20-3401 is a low viscosity system with an extended working time. It is designed for L.E.D. encapsulating, an underfill for flip chips, glob top encapsulation, fiber optics, and any potting or adhesive application requiring clarity. It has excellent adhesion to glass, quartz, most plastics, and metals. 20-3401 passes the Biocompatibility ISO 10993-5 Cytotoxicity Test. The independent lab test report is available upon request. 20-3401 is REACH and RoHS compliant.

Features:

  • Low viscosity
  • Extended working time
  • Outstanding electrical properties
  • Optically clear
  • Packaged in FreezeBond® syringes
  • Passes ISO 10993-5 Cytotoxicity and USP <87>

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccCatalyst
 1.10 g/ccResin
Viscosity 200 - 500 cPMixed
Storage Temperature 75.0 - 85.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82
Shear Strength 2250 psiLap
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm
Dielectric Constant 3.8
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 61.0 µm/m-°CBelow Tg
 180 µm/m-°CAbove Tg
Maximum Service Temperature, Air 150 °C
 300 °CIntermittent
Minimum Service Temperature, Air -45.0 °C
Glass Transition Temp, Tg 80.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.532
Transmission, Visible >= 94 %
@Wavelength 300 nm
 >= 98 %
@Wavelength 1200 - 1600 nm
 >= 99 %
@Wavelength 400 - 1200 nm
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 - 48.0 hour
@Temperature 25.0 °C
 72.0 hour
@Temperature 80.0 °C
Pot Life 480 min
@Load 0.100 kg
Shelf Life 12.0 Month
 
Descriptive Properties
ColorClear
Mix Ratio100:35by weight (Resin:Hardener)
 100:41by volume (Resin:Hardener)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX040 / 316717

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.