High Impact FR Rigid; Rigid polyurethane Key Properties: - Excellent physical properties after post cure
- Low viscosity
- Free of mercury, MOCA, TDI, PBDE, or phthalates
- Excellent impact resistance
- RoHS & REACH compliant
- Meets UL94V0
- Non-Halogenated
Applications: - For hand-batch or meter mix processing
- For short run and prototype parts
Cure 1: 16 hours at 180°FInformation provided by © RAMPF Tooling Solutions GmbH & Co. KG |