MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm ACRYLITE® Resist ZK-M Acrylic polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: ACRYLITE® Resist ZK-M polymer is an amorphous, impact-modified thermoplastic molding and extrusion compound based on polymethyl methacrylate (PMMA).

Typical properties of ACRYLITE® acrylic polymers are:

  • high weather resistance
  • high light transmission
  • improved resistance to stress cracking
  • good melt flow rate
  • easy to color
The special properties of ACRYLITE® Resist ZK-M polymer are:
  • medium impact/break resistance and strength
  • low melt flow rate
  • high heat resistance
  • AMECA listed as ZKM (x)
  • FDA food contact use
Application: Used for injection molded parts.

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Bulk Density 0.710 g/cc0.0257 lb/in³ASTM D1895
Water Absorption <= 0.30 %<= 0.30 %ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 3.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
3.5 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6868ASTM D785
Tensile Strength 58.6 MPa8500 psiASTM D638
Elongation at Break 30 %30 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Tensile Modulus 2.20 GPa319 ksiASTM D638
Flexural Strength 89.6 MPa13000 psiASTM D790
Flexural Modulus 2.20 GPa319 ksiASTM D790
Izod Impact, Notched  0.263 J/cm
@Thickness 6.35 mm,
Temperature >=0.000 °C
0.493 ft-lb/in
@Thickness 0.250 in,
Temperature >=32.0 °F
ASTM D256
 0.449 J/cm
@Thickness 6.35 mm,
Temperature >=23.0 °C
0.841 ft-lb/in
@Thickness 0.250 in,
Temperature >=73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C
@Temperature 0.000 - 100 °C
40.0 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
@Thickness 6.35 mm
196 °F
@Thickness 0.250 in
Annealed; ASTM D648
Vicat Softening Point 210 °C410 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 1.0 %1.0 %ASTM D1003
Yellow Index <= 0.30 %<= 0.30 %ASTM E313
Transmission, Visible >= 91.5 %>= 91.5 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROHM9330 / 319947

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.