MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC XYLEX X8300 PC+Polyester (Europe-Africa-Middle East)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polyester, TP

Material Notes: PC+Polyester, UV Stabilized, Transparent

Information provided by SABIC Innovative Plastics for Europe-Africa-Middle East.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D 792
Density 1.17 g/ccISO 1183
Moisture Absorption 0.200 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 0.050 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 265 °C
ASTM D 1238
 15 g/10 min
@Load 2.16 kg,
Temperature 265 °C
cm^3/10 min Melt Volume Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 73
@Time 10.0 sec
ASTM D 2240
Tensile Strength at Break 46.0 MPaType I, 50 mm/min; ASTM D 638
 54.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 47.0 MPaType I, 50 mm/min; ASTM D 638
 55.0 MPa50 mm/min; ISO 527
Elongation at Break 150 %Type I, 50 mm/min; ASTM D 638
 >= 200 %50 mm/min; ISO 527
Elongation at Yield 5.0 %Type I, 50 mm/min; ASTM D 638
 >= 5.0 %50 mm/min; ISO 527
Tensile Modulus 1520 MPa50 mm/min; ASTM D 638
 1600 MPa1 mm/min; ISO 527
Flexural Strength 78.0 MPa2 mm/min; ISO 178
Flexural Yield Strength 71.0 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 1680 MPa1.3 mm/min, 50 mm span; ASTM D 790
 1700 MPa2 mm/min; ISO 178
Izod Impact, Notched 73.0 J/m
@Temperature -30.0 °C
ASTM D 256
 1120 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature -10.0 °C
80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 10.0 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 95.0 J
@Temperature 23.0 °C
ASTM D 3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D 257
Surface Resistance >= 1.00e+15 ohmASTM D 257
Comparative Tracking Index >= 600 VPLC 0; UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
 105 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 105 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
 105 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 105 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Thermal Conductivity 0.230 W/m-KISO 8302
Hot Ball Pressure Test <= 85.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 80.0 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 75.0 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Vicat Softening Point 91.0 °CRate B/50; ASTM D 1525
 96.0 °CRate B/120; ISO 306
Flammability, UL94 V-2
@Thickness 3.00 mm
UL 94
Glow Wire Flammability Index 750 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.539ISO 489
Haze 1.0 %
@Thickness 2.54 mm
ASTM D 1003
Transmission, Visible 88 %ASTM D 1003

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI49693 / 190778

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.