MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Persian Gulf Polymer HDPE-CC52502
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: CC52502 is a Narrow MWD HDPE specially designed for mineral water bottles and beverage caps. This grade has excellent organoleptic properties which prevent unpleasant odor and taste from cap or closure to transfer to water. It has good gas permeability characteristics, superior process ability and excellent mechanical strength. HDPE CC52502 does not contain slip agent. Application: Caps and closures for mineral water bottles, Caps for sparkling water and carbonated soft drinks, beverage caps. Features: Narrow MWD HDPE, excellent organoleptic property, superior process ability and excellent mechanical strength, good gas permeability characteristics. Additives: HD-CC52502: Antioxidants/Acid scavenger.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 38.0 MPa5510 psiASTM D638
Tensile Strength, Yield 25.0 MPa3630 psiASTM D638
Flexural Modulus 1.00 GPa145 ksiASTM D790
Izod Impact, Notched 1.80 J/cm3.37 ft-lb/inASTM D256/A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C172 °FASTM D648
Vicat Softening Point 124 °C255 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 190 °C320 - 374 °FBarrel Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERSI946 / 250350

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.