BA160E-8229-01 is an impact polypropylene heterophasic copolymer (block copolymer) with optimized mechanical properties, intended for injection molding of compression pipe fittings and is colored black. The product features very good processability. It also shows excellent stress crack resistance and a good resistance to chemicals. BA160E-8229-01 is characterized by a combination of high stiffness and high impact strength, also at low temperatures. BA160E-8229-01 has a ß-crystalline molecular PP structure which improves the mechanical properties as well as the crystallization temperature. This allows for cycle time reduction during injection molding through higher demolding temperatures and shorter cooling time. BA160E-8229-01 is classified as an MRS 8.0 material (PE80). The additive formulation is designed for appropriate durability Applications - BA160E-8229-01 is especially recommended for injection molding of pipe compression fittings/mechanical pipe joints.: - Drinking water
- Irrigation
- Industrial applications
Information provided by Borealis AG |