MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chevron Phillips Marlex® 7105D Polyethylene Film Grade LLDPE Hexene Copolymer
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: This linear low density polyethylene is an ethylene-hexene copolymer tailored for blown film applications that require: • Excellent toughness properties • Good drawdown • Good processing characteristics • Use alone or in co extrusions; blends with other polyolefins

Typical blown film applications include: • High strength industrial film and bags • Thin gauge applications • General purpose packaging.

information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Thickness 25.4 microns1.00 milAs Tested
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 0.000 ppm0.000 ppm
Slip Level 0.000 ppm0.000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 450 %
@Thickness 0.0254 mm
450 %
@Thickness 0.00100 in
ASTM D882
Film Elongation at Break, TD 750 %
@Thickness 0.0254 mm
750 %
@Thickness 0.00100 in
ASTM D882
Coefficient of Friction >= 1.0>= 1.0ASTM D1894
Elmendorf Tear Strength MD 500 g
@Thickness 0.0254 mm
500 g
@Thickness 0.00100 in
ASTM D1922
Elmendorf Tear Strength TD 850 g
@Thickness 0.0254 mm
850 g
@Thickness 0.00100 in
ASTM D1922
Elmendorf Tear Strength, MD 19.7 g/micron
@Thickness 0.0254 mm
500 g/mil
@Thickness 0.00100 in
ASTM D1922
Elmendorf Tear Strength, TD 33.5 g/micron
@Thickness 0.0254 mm
850 g/mil
@Thickness 0.00100 in
ASTM D1922
Dart Drop 15.7 g/micron
@Thickness 0.0254 mm
400 g/mil
@Thickness 0.00100 in
ASTM D1709
Dart Drop Test 400 g
@Thickness 0.0254 mm
0.882 lb
@Thickness 0.00100 in
ASTM D1709
Film Tensile Strength at Break, MD 72.0 MPa
@Thickness 0.0254 mm
10400 psi
@Thickness 0.00100 in
ASTM D882
Film Tensile Strength at Break, TD 52.0 MPa
@Thickness 0.0254 mm
7540 psi
@Thickness 0.00100 in
ASTM D882
1% Secant Modulus, MD 221 MPa
@Thickness 0.0254 mm
32100 psi
@Thickness 0.00100 in
ASTM D882
1% Secant Modulus, TD 262 MPa
@Thickness 0.0254 mm
38000 psi
@Thickness 0.00100 in
ASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 12 %
@Thickness 0.0254 mm
12 %
@Thickness 0.00100 in
ASTM D1003
Gloss 90 %
@Thickness 0.0254 mm
90 %
@Thickness 0.00100 in
60°; ASTM D2457
 
Descriptive Properties
Process AidYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEVC8906 / 241989

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.