MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Zortrax Z-SEMIFLEX Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Z-SEMIFLEX is a material characterized by a minimal shrinkage level and resistance to greases and chemicals. It is based on TPU 98A which gives your models unique characteristics, including high elasticity and rubber-like properties. Z-SEMIFLEX also exhibits high impact strength which allows you to apply force to a 3D printed model with little risk of damage. These unparalleled qualities make Z-SEMIFLEX ideal not only for prototypes tested in adverse industrial environments, but also for models resembling organs used in medical assessment processes.

Information provided by Zortrax

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.176 g/cc0.04249 lb/in³ISO 1183-3:2003
Melt Flow 172.4 g/10 min
@Load 2.16 kg,
Temperature 225 °C
172.4 g/10 min
@Load 4.76 lb,
Temperature 437 °F
ISO 1133:2006
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545ISO 868:1998
Tensile Strength at Break 3.18 MPa461 psiISO 527:1998
Tensile Strength 30.44 MPa4415 psiISO 527:1998
Elongation at Break 543.46 %543.46 %ISO 527:1998
Elongation at Yield 524 %524 %ISO 527:1998
Flexural Strength 5.70 MPa827 psiISO 178:2011
Flexural Modulus 0.09509 GPa13.79 ksiISO 178:2011
Izod Impact, Notched (ISO) 38.88 kJ/m²18.50 ft-lb/in²ISO 180:2004
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 180.16 °C356.29 °FISO 11357-3:2014

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZORT010 / 281889

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.