Butene Copolymer Features: - Good organoleptic properties and natural color
- Outstanding impact and stiffness balance
- High surface gloss
- Exceptional warpage resistance and product performance reliability
Additives: Applications: - Aerosol overcaps
- Caps and closures for non-carbonated beverages
- Housewares
- Frozen food containers
- Seedling trays
- Berry boxes
United States: SCLAIR 2712 resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability. NOVA Chemicals polyethylene resins are biologically and chemically inert. Information provided by NOVA Chemicals® |