Piperazine is a cyclic ethylene amine with two secondary amine groups. Piperazine 68% contains 68% active content diluted with water (PIP-68). Piperazine application fields include pharmaceutical, polyamide, gas sweetening and PU catalysts. CAS number: 110-85-0 EINECS/ELINCS No.: 203-808-3 Information provided by Nouryon |