MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials TIVAR® ECO ESD UHMW-PE, Recycled (ASTM Product Data Sheet)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: This product is a recycled Electro-static dissipating UHMW-PE.

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Key Words: TIVAR® ECO black antistatic UHMW-PE
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 g/ccASTM D792
Water Absorption <= 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67ASTM D2240
Tensile Strength 4000 psiASTM D638
Tensile Strength at 65°C (150°F) 400 psiASTM D638
Elongation at Break 200 %ASTM D638
Tensile Modulus 98.0 ksiASTM D638
Flexural Strength 2000 psiASTM D790
Flexural Modulus 81.0 ksiASTM D790
Compressive Strength 2800 psi10% Def.; ASTM D695
Compressive Modulus 60000 psiASTM D695
Izod Impact, Notched NBASTM D256
Coefficient of Friction, Dynamic 0.14Dry vs. Steel; QTM 55007
Sand Slurry 181018 steel = 100; ASTM D4020
Limiting Pressure Velocity 3000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1e+05 - 1.00e+9 ohmEOS/ESD S11.11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Melting Point 275 °FCrystalline Peak; ASTM D3418
Maximum Service Temperature, Air 180 °FContinuous
Deflection Temperature at 1.8 MPa (264 psi) 116 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA No
NSF No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Conductive / Static Dissipative No
Continuous Sunlight Acceptable
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Limited

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SMP01mV2c / 254067

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.