MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

ALM PA 830-ESD 12 Nylon 11
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Unreinforced

Material Notes: This nylon 11 based material uses graphite for its electrostatic-dissipative (ESD) properties and contains no carbon fibers.

Highlights:

  • Electrostatically dissipative nylon 11 without carbon fibers
  • Good tensile strength and toughness
  • Easy to machine, less abrasive, and excellent surface finish
Applications:
  • Assembly fixtures semiconductor industry
  • Electronic products
  • Applications requiring ESD capabilities

Information provided by Advanced Laser Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.490 g/cc0.0177 lb/in³ASTM D1895
Density 1.10 g/cc0.0397 lb/in³Sintered; ASTM D792
Particle Size 55 µm55 µmD50
 31 - 95 µm31 - 95 µmD10-D90
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 29.0 MPa4210 psiASTM D638
Elongation at Break 8.0 %8.0 %XY; ASTM D638
Tensile Modulus 2.944 GPa427.0 ksiXY; ASTM D638
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 2400 ohm2400 ohmTop Facing Surface O; ASTM D257
 33000 ohm33000 ohmBottom Facing Surface O; ASTM D257
 
Descriptive Properties
ColorBlack with Silver Flakes
Melt ViscosityVirgin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALP9007 / 312342

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.