MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

Special Metals MONEL® Alloy 400
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chemical and hydrocarbon processing equipment, valves, pumps, shafts, fittings, fasteners, and heat exchangers. Standard product forms are round, hexagon, flats, forging stock, pipe, tube, plate, sheet, strip, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: AFNOR NU30; SAE AMS 4544, 4574, 4575, 4675, 4730, 4731, 7233; DIN 17743, 17750 - 17754, ASME SB-127, SB-163 - SB-165, SB-564, Boiler Code Sections III, IV, VIII, IX; AECMA Pr EN 2305, Monel Nickel-Copper Alloy, UNS N04400; BS 3072-3076 (NA 13); ASTM B 127, B 163 - B 165, B 564, Werkstoff Nr. 2.4360, 2.4361; VdTUV 263; MIL-T-1368, MIL-T-23520, MIL-N-24106; QQ-N-281; NACE MR-01-75
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 550 MPa79800 psiAnnealed
 450 MPa
@Temperature 425 °C
65300 psi
@Temperature 797 °F
Annealed prior to test
Tensile Strength, Yield 240 MPa34800 psiAnnealed
 170 MPa
@Temperature 425 °C
24700 psi
@Temperature 797 °F
Annealed prior to test
Elongation at Break 48 %48 %Annealed prior to test.
 50 %
@Temperature 425 °C
50 %
@Temperature 797 °F
Annealed prior to test.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000547 ohm-cm0.0000547 ohm-cm
Curie Temperature 20.0 - 50.0 °C68.0 - 122 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.9 µm/m-°C
@Temperature 20.0 - 100 °C
7.72 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.427 J/g-°C0.102 BTU/lb-°F
Thermal Conductivity 21.8 W/m-K151 BTU-in/hr-ft²-°F
Melting Point 1300 - 1350 °C2370 - 2460 °F
Solidus 1300 °C2370 °F
Liquidus 1350 °C2460 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.30 %<= 0.30 %
Copper, Cu 28 - 34 %28 - 34 %
Iron, Fe <= 2.5 %<= 2.5 %
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni >= 63 %>= 63 %Including Cobalt
Silicon, Si <= 0.50 %<= 0.50 %
Sulfur, S <= 0.024 %<= 0.024 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals MONEL® Alloy K-500
Special Metals MONEL® Alloy R-405
Special Metals MONEL® Alloy 401
MetalTek MTEK A Cast UNS N04020 Nickel-Copper Alloy
Special Metals MONEL® 404 Copper-Nickel Alloy

NINC10 / 17393

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.