MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
ITW Insulcast® 116 FR-FC Epoxy Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. INSULCAST 116 FR-FC is a one to one ratio (weight or volume) epoxy potting and casting compound designed for production use. The convenient mixing ratio makes it ideal for production line mixing as well as automatic dispensing. The IINSULCAST 116 FR-FC is among the safest epoxy compounds available. It appreciably reduces the risk of eye, skin or respiratory problems generally associated with the use of epoxy compounds.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccUncured. Part A
 1.50 g/ccUncured. Part B
Viscosity 7200 cPPart A; ASTM D2393
 9800 cPUncured, mixed
 11000 cPUncured. Part B; ASTM D2393
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65 - 75ASTM D2240
Tensile Strength 9500 psiASTM D638
Elongation at Break 5.0 - 7.0 %ASTM D638
Flexural Strength 10000 psiASTM D790
Compressive Strength 11500 psiASTM D695
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Constant 4.4
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 420 V/milASTM D149
Dissipation Factor 0.020
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µm/m-°C
Thermal Conductivity 4.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 105 °C
Heat Distortion Temperature 80.0 °CLoad Not Reported
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Pot Life 30.0 - 45.0 min150 grams
Gel Time 60.0 - 120 min
@Temperature 25.0 °C
Shelf Life 12.0 Month
 
Descriptive Properties
ColorBlackUncured. Part A
 NeutralUncured. Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWIN9097 / 239607

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.