MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® G-501NK Diamine Terpolymer
Categories: Polymer

Material Notes: Good mechanical characteristics

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.93 g/cc
Mooney Viscosity 74
@Temperature 121 °C
ML1+10
 110
@Temperature 100 °C
ML1+10
 136
@Temperature 100 °C
Compound, ML1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75peak
 69
@Time 3.00 sec
 76
@Treatment Temp. 230 °C,
Time 252000 sec
Air aging test
 79
@Treatment Temp. 250 °C,
Time 252000 sec
Air aging test
 81
@Treatment Temp. 275 °C,
Time 252000 sec
Air aging test
Tensile Strength at Break 17.4 MPa
 10.4 MPa
@Treatment Temp. 275 °C,
Time 252000 sec
Air aging test
 11.4 MPa
@Treatment Temp. 250 °C,
Time 252000 sec
Air aging test
 14.9 MPa
@Treatment Temp. 230 °C,
Time 252000 sec
Air aging test
Elongation at Break 280 %
 244 %
@Treatment Temp. 275 °C,
Time 252000 sec
Air aging test
 266 %
@Treatment Temp. 250 °C,
Time 252000 sec
Air aging test
 308 %
@Treatment Temp. 230 °C,
Time 252000 sec
Air aging test
100% Modulus 4.10 MPa
@Strain 100 %
Tear Strength 45.0 kN/mangle type
Compression Set 28 %
@Temperature 100 °C,
Time 252000 sec
P-24 O-ring
 35 %
@Temperature 150 °C,
Time 252000 sec
P-24 O-ring
 45 %
@Temperature 50.0 °C,
Time 252000 sec
P-24 O-ring
 50 %
@Temperature 175 °C,
Time 252000 sec
P-24 O-ring
 65 %
@Temperature 25.0 °C,
Time 252000 sec
P-24 O-ring
 65 %
@Temperature 200 °C,
Time 252000 sec
P-24 O-ring
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -16.0 °CLow Temperature Retraction, TR10
 -15.0 °CGehman Torsion T10
 -9.00 °CGehman Torsion T2
 -8.00 °CLow Temperature Retraction, TR70
Brittleness Temperature -31.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Temperature 160 °C
Curelastometer, T90
 6.00 min
@Temperature 160 °C
MDR, T90
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 68 %
 
Descriptive Properties
Test Formula100Polymer
 15MgO
 20N990 Carbon Black
 3Curing Agent V-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDAIJ9941 / 210014

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.