MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Syensqo (Solvay Specialty Polymers) Ryton® R-7-150BL PPS, Glass fiber and mineral filled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Ryton® R-7-150BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.

Features: Chemical Resistant; Good Electrical Properties; Good Strength

Test specimen molding conditions: Stock temperature, 315-345°C; Mold temperature, 135°C

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.95 g/cc0.0704 lb/in³Method A; ISO 1183
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 165 MPa23900 psiASTM D638
Elongation at Break 1.1 %1.1 %ASTM D638
Flexural Strength 255 MPa37000 psiASTM D790
Flexural Modulus 19.0 GPa2760 ksiISO 178
Compressive Strength 300 MPa43500 psiASTM D695
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²Notch A; ISO 180
Izod Impact, Unnotched (ISO) 25.0 kJ/m²11.9 ft-lb/in²ISO 180
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Insulation Resistance 1.00e+13 ohm
@Temperature 90.0 °C
1.00e+13 ohm
@Temperature 194 °F
Dielectric Constant  5.1
@Frequency 1000 Hz
5.1
@Frequency 1000 Hz
ASTM D150
 5.1
@Frequency 1e+6 Hz
5.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm457 kV/inASTM D149
Dissipation Factor  0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 185 sec185 secASTM D495
Comparative Tracking Index 150 V150 VUL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  10.0 µm/m-°C
@Temperature 100 - 200 °C
5.56 µin/in-°F
@Temperature 212 - 392 °F
ISO 11359-2
 15.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F
@Temperature -58.0 - 122 °F
ISO 11359-2
CTE, linear, Transverse to Flow  30.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
16.7 µin/in-°F
@Temperature -58.0 - 122 °F
ISO 11359-2
 75.0 µm/m-°C
@Temperature 100 - 200 °C
41.7 µin/in-°F
@Temperature 212 - 392 °F
ISO 11359-2
Thermal Conductivity 0.530 W/m-K3.68 BTU-in/hr-ft²-°FISO 8302
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4447 / 280247

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.