MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Excelite Plastic Acrylic Sheet
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Excelite Acrylic has both casting and extrusion processing equipment. The products have super excellent transparency, excellent weather ability, good processing properties, and excellent overall performance.

Features:

  • Excellent transparency, transmittance 92%
  • Excellent weather ability
  • Antiaging properties performance
  • Good processing properties for both machining and thermo forming
  • 10 years warranty
  • ease of cleaning
Potential Applications:
  • Sound Barrier
  • Skylight
  • Light box, Lampshade
  • Signs
  • Display Stand
  • Protective mask
  • Crystal Furniture
  • Bathtub
  • Aquarium
  • Light guide plate

Information provided by Excelite Plastic Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 - 1.20 g/cc
Thickness 1500 - 2000 micronsExtrusion sheet
 2000 - 50000 micronsCasting Sheet
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 100
Tensile Strength 760 kg(f)/cm²
Flexural Strength 103 MPa
Compressive Strength 1260 kg(f)/cm²
Shear Strength 61.8 MPa
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+16 ohm
Dielectric Strength 20.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
Specific Heat Capacity 1.46 J/g-°C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 92 %
 
Descriptive Properties
ColorClearExtrusion sheet
 ClearCasting Sheet
Deformation Temp100°C
Thermo Forming Temp140-180°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Cast
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
Esstech X-127-0950 Poly Methyl Methacrylate
Overview of materials for Acrylic, Optical Sheet
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade

PEXLT001 / 198711

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.