A High Performance Sponge Polymer Unique Features: - Very high Molecular weight
- Ultra fast curing
- Improved abrasion resistance
- High tensile strength and high tear resistance
- High wrinkle resistance while maintaining soft compression deflection
- Excellent green strength for extruded profile shape stability
- Rapid Banbury mixing and excellent dispersion properties
- Extended with a white, hydrotreated paraffinic oil
Applications: - TPO and TPV
- Automotive closed cell sponge extrusions and molded sponge corners
- Closed cell sheet sponge
- Dynamic applications
Information provided by Lion Elastomer |