MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Alliance BIN-12 Injection Molded NdFeB Magnet
Categories: Ceramic; Oxide; Metal; Electronic/Magnetic Alloy

Material Notes: Injection Molded NdFeB Magnets are made by combining NdFeB powders with Nylon 6, Nylon 12, PPS and other resins. The ratios between magnetic powders and resins are variable, therefore many grades exist depending on magnetic performance, temperature resistance, and mechanical strength. These materials can be molded directly over or into another polymer or metal component. The shapes and sizes are also adjustable, as are the magnetization patterns that can be achieved either in the molding tool or by utilizing a magnetizing fixture.

Information provided by Alliance LLC.

Key Words: Permanent Magnet
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.40 - 4.80 g/cc
Water Absorption 0.020 - 0.050 %PPS
 0.050 - 3.2 %PA12
 0.30 - 11 %PA6
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 80 - 130
Tensile Strength, Yield 20.0 - 140 MPaPA6
 15.0 - 150 MPaPPS
 12.0 - 170 MPaPA12
 
Electrical PropertiesOriginal ValueComments
Magnetic Coercive Force, Hc 3830 Oe
 8680 OeIntrinsic
Magnetic Remanence, Br 4540 Gauss
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air <= 120 °CPA12
 <= 150 °CPA6
 <= 170 °CPPS
 
Processing PropertiesOriginal ValueComments
Mold Temperature 60.0 - 100 °CPA12
 70.0 - 120 °CPA6
 120 - 150 °CPPS
 
Descriptive Properties
Reversible Temperature Coefficients-0.12Bd. %/°C
 -0.43Hd. %/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NALLIAN9892 / 268428

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.