MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical LUTENE® XL8080UCS XLPE
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Applications: Cross-linkable polyethylene compound for high and extra high voltage power cable insulation with rated voltage up to 230kV

LUTENE® XL8080UCS is a superior cleanliness version for high and extra high voltage power cable insulation and is designated as UC (Ultra-Clean) due to its extremely low level of contamination.

Specification: LUTENE® XL8080UCS meets the property requirement of the following material specifications.
? AEIC CS9
? AEIC CS8
? KSC 3611
? ICEA S-94-649
? IEC 60502
? IEC 60840
? IEC 62067

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccBase Resin; ASTM D1505
Deformation <= 15 %
@Pressure 0.200 MPa,
Temperature 200 °C
Permanent, Hot Set Test; IEC 60811-2-1
Degree of Crosslinking >= 80 %ASTM D2765A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 19.7 MPa200 mm/min; ASTM D638
 >= 17.7 MPa
@Treatment Temp. 135 °C,
Time 605000 sec
retention after; ASTM D638
Elongation at Break >= 500 %200 mm/min; ASTM D638
 >= 450 %
@Treatment Temp. 135 °C,
Time 605000 sec
retention after; ASTM D638
Tensile Set <= 175 %
@Treatment Temp. 200 °C,
Pressure 0.200 MPa
Elongation, Hot Set Test; IEC 60811-2-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmDC; ASTM D257
Dielectric Constant 2.25
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength >= 22.0 kV/mmASTM D149
Dissipation Factor 0.00060
@Frequency 1e+6 Hz
ASTM D150

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLHCHEM9893 / 239409

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.