MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecapeek® IM GF30 natural Polyetheretherketone, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes:
  • good heat deflection temperature
  • very good chemical resistance
  • very high creep resistant
  • hydrolysis and superheated steam
  • resistant
  • inherent flame resistance
  • very high stiffness
  • high dimensional stability
  • resistance against high energy radiation
Target Industries:
  • aircraft and aerospace technology
  • aircraft and aerospace interiors
  • food engineering
  • food processing
  • agricultural machinery
  • automotive industry
  • electrical engineering
  • chemical plant engineering
  • mechanical engineering
  • conveyor technology

Information provided by Ensinger Inc.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³
Moisture Absorption 0.110 %
@Time 86400 sec
0.110 %
@Time 24.0 hour
ASTM D 570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 157 MPa22800 psiASTM D 638
Elongation at Break 2.2 %2.2 %ASTM D 638
Modulus of Elasticity 9.6995 GPa1406.8 ksi1% Sec; ASTM D 638
Flexural Strength 233 MPa33800 psiASTM D 790
Flexural Modulus 10.309 GPa1495.2 ksiASTM D 790
Compressive Strength 215 MPa31200 psiASTM D 695
Shear Strength 97.2 MPa14100 psi
Izod Impact, Notched 0.961 J/cm1.80 ft-lb/inASTM D 256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.6 µm/m-°C12.0 µin/in-°FASTM D 696
Thermal Conductivity 0.432 W/m-K3.00 BTU-in/hr-ft²-°F
Melting Point 334 °C633 °F
Maximum Service Temperature, Air 260 °C500 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 316 °C
@Thickness 6.35 mm
600 °F
@Thickness 0.250 in
ASTM D 648
Flammability, UL94 V-0V-0
 
Descriptive Properties
Colornatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8182 / 319110

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.