MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Huber MoldX® A300 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: MoldX® A300 optimized alumina trihydrate (ATH) was designed specifically to provide dramatically improved processing viscosities to sheet molding compounds (SMC) at loadings ranging from 250 phr to greater than 350 phr. The unique characteristics of MoldX® A300 optimized ATH makes it our highest performing “low viscosity” grade. The high loading levels allow for the elimination of halogenated resins and additives typically used to pass conventional flame-retardant certification tests such as UL 94V-O, UL94 5VA, Dockett 90, or ASTM E84 Class A ratings. The elimination of halogens from SMC formulations result in greatly reduced smoke generation, allowing compounds to pass UL 723. MoldX® A300 can also be used to achieve low-cost flame retardancy and smoke suppression in a variety of other color sensitive thermoset processes such as bulk molding compounds (BMC), spray-up, hand lay-up, and wet-mat molding.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.42 g/cc
Bulk Density 0.860 g/ccloose
Brightness 91 %TAPPI
Moisture Absorption 0.200 %
@Temperature 105 °C
Free
Particle Size >= 10 µmMedian Particle Diameter
 <= 10 µm52 percent
Particle Mesh Size 325 Mesh62% through
Specific Surface Area 1.8 m²/gBET
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 0.0070 %
Loss on Ignition(%) 34.6 %
@Temperature 1000 °C
Na2O 0.025 %soluble
 0.20 %total
SiO2 0.0050 %
 
Descriptive Properties
Al(OH)3 (%)99.6
FunctionalityRapid Dispersion
 Smoke Suppression
Market/Application: ThermosetsSMC/BMC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EHUBER752 / 300858

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.