MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Radici Heraflex® E 5620 TPC-ET Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: TPC-ET Thermoplastic Elastomer. Medium Modulus, Nominal Shore D/15s 50. Natural color

Processing technology: Injection molding

Information provided by Radici group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/cc
Water Absorption 0.29 %
@Time 86400 sec
MI / 08
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 56Instantaneous; ISO 868
 50
@Time 15.0 sec
ISO 868
Tensile Strength at Break 43.0 MPaISO 527-1/2
Elongation at Break 688 %ISO 527 1/2
Flexural Modulus 221 MPaISO 178/1A
Izod Impact, Notched NBASTM D256
Tear Strength 174 kN/mASTM D1004
Abrasion 15mm3; DIN 53516
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
Melting Point 199 °C
Vicat Softening Point 177 °C
@Load 5.10 kg
50°C/h
Flammability, UL94 HB
@Thickness 1.60 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® G3548 NC010 TPC-ET
Celanese Riteflex® 425 TPC, Unfilled
Radici Heraflex® E 3918 TPC-ET Thermoplastic Elastomer
Envalior Arnitel® EM631-HB TPC-ET
Celanese Riteflex® XFR 655 TPC, Unfilled

PRADI752 / 120265

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.