MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil ExxonMobil™ AXO3BE3 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: A high crystallinity, medium impact copolymer resin designed for injection-molded automotive interior applications and large appliance parts applications requiring high melt flow rate and excellent processing attributes. 

Availability:  North America.  Features:  fast molding cycle, good stiffness, nucleated, good flow, impact modified. 

Applications:  appliances, automotive interior parts, consumer applications, automotive applications, compounding, industrial applications.  Appearance:  natural color.  Forms: pellets.  Processing Method:  injection molding.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccExxonMobil Method
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3670 psi2.0 in/min; ASTM D638
Elongation at Yield 4.4 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 203000 psi0.051 in/min; ASTM D790A
 232000 psi0.51 in/min; ASTM D790B
Izod Impact, Notched 0.800 ft-lb/in
@Temperature -17.8 °C
ASTM D 256A
 1.40 ft-lb/in
@Temperature 22.8 °C
ASTM D 256A
Charpy Impact, Notched 2.10 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 2.10 ft-lb/in²
@Temperature -20.0 °C
ISO 179/1eA
 2.40 ft-lb/in²
@Temperature 0.000 °C
ISO 179/1eA
 3.70 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
Gardner Impact 169 in-lb
@Thickness 3.17 mm,
Temperature -28.9 °C
geometry GC; ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 208 °FISO-75-2/Bf
Deflection Temperature at 1.8 MPa (264 psi) 131 °FISO-75-2/A
 
Descriptive Properties
Rockwell Hardness91ASTM D785

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil PP7035E5 Impact Copolymer
LyondellBasell Moplen RP348SK Polypropylene Copolymer
LyondellBasell Pro-fax SV956 Polypropylene Copolymer
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade
ExxonMobil PP9074MED Polypropylene Homopolymer

PEX98975 / 238356

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.