MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Bayport Polymers Baystar™ HL 535 High Density Polyethylene, Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Medium molecular weight, high density film resin

Characteristics:

  • High stiffness
  • Good heat resistance
  • Excellent bubble stability
  • Good compatibility with LDPE and LLDPE

Applications:

  • Release liners
  • Stand-up bags
  • Coextruded films

This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D-792
Water Vapor Transmission 0.700 g/100 in²/day
@Temperature 37.8 °C
ASTM F-1294
Melt Flow 0.35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D-1238
High Load Melt Index 30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 4000 psiASTM D882, A, 20 in/min
Film Tensile Strength at Yield, TD 4300 psiASTM D882, A, 20 in/min
Film Elongation at Break, MD 500 %ASTM D-882, A, 20 in/min
Film Elongation at Break, TD 25 %ASTM D-882, A, 20 in/min
Elmendorf Tear Strength MD 8.0 gASTM D-1922
Elmendorf Tear Strength TD 1100 gASTM D-1922
Dart Drop Test <= 50.0 gASTM D-1709, A
Film Tensile Strength at Break, MD 6300 psiASTM D-882, A, 20 in/min
Film Tensile Strength at Break, TD 4300 psiASTM D-882, A, 20 in/min
1% Secant Modulus, MD 133000 psiASTM D-882, A, 20 in/min
1% Secant Modulus, TD 186000 psiASTM D-882, A, 20 in/min
 
Thermal PropertiesOriginal ValueComments
Melting Point 270 °FASTM D-3417
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 420 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Reliance Industries Relene E52009 Polyethylene
Formosa Plastics Formolene® LH5204 Injection Molding HDPE
Total HT 514 MDPE film
Total HD 6081 High Density Polyethylene - Injection Molding
Total Finathene® 2344 HDPE film

PBAYST821 / 130476

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.