MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Pressure Seal 55904 Nitrile - Butadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 55904 is a 90 durometer black colored Highly Saturated Nitrile (HNBR) elastomer, it is formulated for high temperature applications. It exhibits good resistance to petroleum based oils and sour crude.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 6 BG 915 A14 B14 B34 EO14 EO34; 7 BG 915 B14 EO14 EO34 EF11 EF21 EA14 F16; M 4 BK 910 A24 B14 B34 EF11 EO14; 3 CH 915 A25 B14 B34 EO16 EO36; 4 CH 915 A25 B14 EO15 EO35 EF31 F16; 5 CH 915 A25 B14 B34 F14; 6 CH 915 A25 B14 B34 EO36; 4 DH 929 B36 EO16 EO36; M 4 DH 920 B36 EO16 EO36

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 91
 77
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 79
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 87
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 87
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 87
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 90
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 90
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 91
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 92
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 92
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 93
@Temperature 100 °C,
Time 252000 sec
Heat Aged
 93
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 93
@Temperature 100 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 95
@Temperature 150 °C,
Time 252000 sec
Heat Aged
Tensile Strength 3107 psi
 1861.1 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 2056.8 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 2873.98 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 2985.8 psi
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 2992.1 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 3029.3 psi
@Temperature 100 °C,
Time 252000 sec
Heat Aged
 3029.3 psi
@Temperature 100 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 3184.7 psi
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 3268.6 psi
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 3327.6 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 3349.3 psi
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 3352.45 psi
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 3439.5 psi
@Temperature 150 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 158 %
 94.6 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 107 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 121.1 %
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 121.66 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 134 %
@Temperature 100 °C,
Time 252000 sec
Heat Aged
 139.99 %
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #3 (IRM 903)
 149 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 149.8 %
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 152.3 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 154.05 %
@Temperature 100 °C,
Time 252000 sec
Heat Aged, Test Tube Method
 170.3 %
@Temperature 125 °C,
Time 252000 sec
ASTM Oil #1 (IRM 901)
 170.5 %
@Temperature 125 °C,
Time 252000 sec
Heat Aged
 174.9 %
@Temperature 150 °C,
Time 252000 sec
Heat Aged
50% Modulus 1171 psi
100% Modulus 2355 psi
Tear Strength 215 pliDie B
 242 pliDie C
Compression Set 8.4 %
@Temperature 100 °C,
Time 79200 sec
Solid
 9.1 %
@Temperature 125 °C,
Time 79200 sec
Solid
 11.4 %
@Temperature 100 °C,
Time 252000 sec
Solid
 13 %
@Temperature 100 °C,
Time 79200 sec
Plied
 14 %
@Temperature 125 °C,
Time 79200 sec
Plied
 14 %
@Temperature 100 °C,
Time 252000 sec
Plied
 17 %
@Temperature 150 °C,
Time 79200 sec
Plied
 31.2 %
@Temperature 150 °C,
Time 79200 sec
Solid
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -35.0 °F
Shrinkage -2.10 %
@Temperature 125 °C,
Time 252000 sec
Volume, ASTM Oil #1
 -2.10 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #1
 -2.00 %
@Temperature 100 °C,
Time 252000 sec
Volume, ASTM Oil #1
 1.2 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel A
 1.4 %
@Temperature 100 °C,
Time 252000 sec
Volume, Distilled water aged
 8.9 %
@Temperature 100 °C,
Time 252000 sec
Volume, ASTM Oil #3
 9.3 %
@Temperature 125 °C,
Time 252000 sec
Volume, ASTM Oil #3
 10.3 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #3
 28.6 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel B
 46 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel C
 
Descriptive Properties
ColorBlack
TR-10 Temperature-29°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL057 / 318267

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.