MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials HiDura™ D1XA NT Nylon PA612
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: HiDura D1XA NT is a low-medium viscosity PA612 grade. It is suitable for monofilament, film and general purpose injection molding applications. It exhibits low moisture absorption, good chemical resistance, dimensional stability and high impact resilience. PA612 offers a unique balance of thermal, mechanical and physical properties.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccDAM; ISO 1183
Water Absorption 0.40 %
@Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.3 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.019 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 44.0 MPaDAM; ISO 527-2
 63.0 MPa50% RH; ISO 527-2
Tensile Strength, Yield 54.0 MPa50% RH; ISO 527-2
 60.0 MPaDAM; ISO 527-2
Elongation at Break >= 50 %50% RH; ISO 527-2
 >= 50 %DAM; ISO 527-2
Elongation at Yield 4.4 %DAM; ISO 527-2
 19 %50% RH; ISO 527-2
Tensile Modulus 1500 MPa50% RH; ISO 527-2
 2100 MPaDAM; ISO 527-2
Flexural Strength 39.0 MPa50% RH; ISO 178
 68.0 MPaDAM; ISO 178
Flexural Modulus 1500 MPa50% RH; ISO 178
 2200 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 4.10 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 4.40 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 4.80 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 5.10 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 5.10 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 5.20 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -40.0 °C
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 5.20 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 5.30 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 5.60 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 5.70 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 5.70 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 7.20 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 30.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 30.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 120 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 136 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 218 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 136 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °CUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 275 °CInjection
Middle Barrel Temperature 265 - 280 °CInjection
Front Barrel Temperature 265 - 290 °CInjection
Nozzle Temperature 265 - 290 °CInjection
Zone 1 240 - 260 °CExtrusion
Zone 2 240 - 260 °CExtrusion
Zone 3 240 - 260 °CExtrusion
Zone 4 240 - 260 °CExtrusion
Zone 5 240 - 260 °CExtrusion
Die Temperature 240 - 260 °CExtrusion
Melt Temperature 230 - 255 °CExtrusion
 230 - 290 °CInjection
Mold Temperature 50.0 - 100 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 - 6.00 hourInjection
Moisture Content 0.15 %Injection
 
Descriptive Properties
AppearanceNatural Color
FeaturesAbrasion Resistance
 Chemical Resistant
 Medium Viscosity
FormsPellets
Processing MethodCasting
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8601 / 293350

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.