MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Danquinsa DANCURE® 999 Isocyanate Hardeners
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANCURE® 999 is a poly functional isocynate in powder form. This isocyanate powder serves for the curing of polyurethane- and Polycaprolactone based thermoplastic adhesive powders. By the curing of adhesive powders, a higher heat resistance as well as a better chemical resistance of the adhesive bonding is obtained. Immediately after the powder production DANCURE® 999 can be added to the thermoplastic adhesive powders for curing purposes. As long as the product is stored at a temperature below 50° C, there is no reaction. A reaction with DANCURE® 999 takes place in a temperature range between 80 to 180°C. Optimum curing temperatures are between 90 - 130° C. Even the production of 1KPUR- dispersion systems is possible with DANCURE® 999 isocyanate powder.

Application: As a curing agent, DANCURE® 999 is mixed to thermoplastic adhesives in powder form. The addition to the powder adhesive materials will be 3 to 10% to DANCURE® 999. Also the cross linking of OH-group based and aqueous adhesive dispersions or adhesive powder dispersion pastes is possible with DANCURE® 999. The amount of DANCURE® 999 added in aqueous systems is in the range of 3 to 8 percent by weight. Such aqueous solvable 1K-dispersion adhesive materials have a good storage ability. They will cross link only during the adhesive application.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccDIN 51.757
Solids Content 100 %DIN 53.189
Storage Temperature 10.0 - 30.0 °C
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 380 °CDIN 51.755
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Aspectwhite, fine and regular (homogeneous) powder
Chemical compositionpolyfunctional isocyanate powder
Composition<0.15%Residual monomer content
 47-49%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ110 / 294530

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.