(Viewing data as-entered.
Click here
to return)
Osterman & Co Osterlene® LLH2018 LLDPE
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Linear Low Density (LLDPE)
Material Notes:
Product Description: LLH2018 has exceptional toughness and low gel level. Applications for LLH2018 include cast stretch wrap.
Availability: North America
Features: Good Toughness; Low Gel
Uses: Stretch Wrap
Information provided by Osterman & Company
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.918
g/cc
ASTM D1505
Melt Flow
2.0
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Puncture Resistance
17.3
lb (f)
ASTM D3763
Film Tensile Strength at Yield, MD
1500
psi
ASTM D882
Film Tensile Strength at Yield, TD
1500
psi
ASTM D882
Film Elongation at Break, MD
500 %
ASTM D882
Film Elongation at Break, TD
780 %
ASTM D882
Secant Modulus, MD
21.8
ksi
ASTM D790
Secant Modulus, TD
24.7
ksi
ASTM D790
Puncture Energy
55.6
in-lb
ASTM D3763
Coefficient of Friction
>= 1.0
ASTM D1894
Elmendorf Tear Strength MD
260
g
ASTM D1922
Elmendorf Tear Strength TD
420
g
ASTM D1922
Dart Drop Test
100
g
ASTM D1709
Film Tensile Strength at Break, MD
5700
psi
ASTM D882
Film Tensile Strength at Break, TD
4200
psi
ASTM D882
Optical Properties
Original Value
Comments
Haze
2.0 %
ASTM D1003
Gloss
90 %
45°; ASTM D2457
Descriptive Properties
Dart Impact
>1500 lbf/in
ASTM D1709
Sealing Initial Temperature
216°F
ASTM F88
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
POSTER115 / 267697
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.