MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow Agility™ 1023 Performance LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Product Description: Agility 1023 Performance LDPE is used in clarity packaging with good stiffness neat and in blends with LLDPE for industrial and food packaging applications.
Main Characteristics:
  • High optics for sparkling packages
  • Good stiffness
  • Excellent processability
Complies with: US FDA 21 CFR 177.1520 ©2.2; EU No 10/2011. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520 ©2.2; EU No 10/2011

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 13.5 MPa
@Thickness 0.0330 mm
1960 psi
@Thickness 0.00130 in
ASTM D882
Film Tensile Strength at Yield, TD 13.5 MPa
@Thickness 0.0330 mm
1960 psi
@Thickness 0.00130 in
ASTM D882
Film Elongation at Break, MD 330 %330 %0.0013; ASTM D882
Film Elongation at Break, TD 550 %550 %0.0013; ASTM D882
2% Secant Modulus  0.207 GPa
@Thickness 0.0330 mm
30.0 ksi
@Thickness 0.00130 in
MD; ASTM D882
 0.234 GPa
@Thickness 0.0330 mm
34.0 ksi
@Thickness 0.00130 in
TD; ASTM D882
Elmendorf Tear Strength MD 280 g280 g0.0013; ASTM D1922
Elmendorf Tear Strength TD 300 g300 g0.0013; ASTM D1922
Dart Drop Test 66.0 g
@Thickness 0.0330 mm
0.146 lb
@Thickness 0.00130 in
ASTM D1709A
Film Tensile Strength at Break, MD 21.6 MPa
@Thickness 0.0330 mm
3130 psi
@Thickness 0.00130 in
ASTM D882
Film Tensile Strength at Break, TD 17.0 MPa
@Thickness 0.0330 mm
2460 psi
@Thickness 0.00130 in
ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 112 °C234 °F
 
Optical PropertiesMetricEnglishComments
Haze 5.4 %
@Thickness 0.0317 mm
5.4 %
@Thickness 0.00125 in
ASTM D1003
Gloss 78 %
@Thickness 0.0317 mm
78 %
@Thickness 0.00125 in
45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 212 °C413 °FExtrusion
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
Film Puncture Resistance45 ft-lb/in31.3 mil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF388 / 311081

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.