MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis RJ908MO Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: RJ908MO is a transparent polypropylene random ethylene copolymer with high melt flow. This clarified product is designed for high speed injection molding at low temperature and contains antistatic additives. This polymer has a narrow molecular weight distribution giving low warpage. Products originating from this grade have excellent transparency and gloss, and good balance of stiffness and impact strength at ambient temperatures. Cas No. 9010-79-1

Special Features:

  • Excellent flow behavior
  • Excellent processability
  • Very good optical properties
  • Good clarity
  • Good gloss
  • Good stiffness and impact balance
Applications:
  • Articles with rather long and narrow flow lengths
  • Products with complicated geometry
  • Transparent storage crates and boxes (House wares)
  • Lids
  • Square containers

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccISO 1183
Melt Flow 80.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 1150 MPa1 mm/min; ISO 527-2
Flexural Modulus 1100 MPaISO 178
Charpy Impact, Notched 4.20 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CISO 75-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9907 / 323264

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.