MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECACOMP POM TRM natural 1064527 POM-C, Silicone Oil/PTFE Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, PTFE Filled

Material Notes:
  • very good bearing and wear properties
Target Industries:
  • automotive industry
  • mechanical engineering

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³
Water Absorption at Saturation 0.20 %0.20 %50 % relative humidity up to saturation; DIN EN ISO 62
Linear Mold Shrinkage, Flow 0.028 cm/cm0.028 in/inDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.023 cm/cm0.023 in/inDIN EN ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 59.0 MPa8560 psiDIN EN ISO 527-1
Elongation at Break 24 %24 %DIN EN ISO 527-1
Modulus of Elasticity 2.50 GPa363 ksiDIN EN ISO 527-1
Charpy Impact Unnotched 0.800 J/cm²3.81 ft-lb/in²DIN EN ISO 179-1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmDIN EN 61340-2-3
Surface Resistance 1.00e+13 ohm1.00e+13 ohmDIN EN 61340-2-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 175 °C347 °F
Maximum Service Temperature, Air 110 °C230 °Flong term
 150 °C302 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °FISO-R 75 Method A
Glass Transition Temp, Tg -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 220 °C356 - 428 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 100 °C212 °F
Dry Time 4.00 - 8.00 hour4.00 - 8.00 hour
 
Descriptive Properties
Colornatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO9112 / 319040

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.