MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LG Chemical NBR 2875 High Acrylonitrile Polymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: NBR 2875 is a copolymer of butadiene and acrylonitrile to be manufactured by cold emulsion polymerization through the advanced technology and process of LG Chem. NBR 2875 is a non staining, high Mooney, and medium low acrylonitrile polymer designed to aid in processing operations such as extrusion and press molding. And also, this grade offers good flexibility and elasticity in low temperature by the minimized block structure on polymer chain. NBR 2875 is preferably used for industrial and automotive hoses and many rubber parts such as roller, gasket and o-rings. And also, it can be used for foam insulation application due to excellent elasticity and good flexibility in low temperature.

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/cc
Volatiles 0.20 %
Mooney Viscosity 75
@Temperature 100 °C
ML1+4
Ash 0.50 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 290 kg(f)/cm²145°C×50min. Cured; ASTM D412
Elongation at Break 435 %145°C×50min. Cured; ASTM D412
300% Modulus 190 kg(f)/cm²
@Strain 300 %
145°C×50min. Cured; ASTM D412
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
@Temperature <=30.0 °C
 
Descriptive Properties
Bound AN Content (%)28
ColorLight Tan
StabilizerNon-Staining

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLHCHEM9851 / 239367

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.