MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Elements Manganese Oxide Nanopowder
Categories: Ceramic; Oxide

Material Notes: General Description

Manganese Oxide Nanopowder (MnO), nanodots or nanoparticles are high surface area particles. Nanoscale Manganese Oxide Nanoparticles are typically 5 - 100 nanometers (nm) with specific surface area (SSA) in the 25 – 50 m 2 /g range. Nano Manganese Oxide Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Manganese oxide nanocrystals include to absorb radionucleotides, as a Magnetic Nanoparticle (also in iron oxide -manganese oxide nanoparticles) for magnetic data storage and magnetic resonance imaging (MRI), in biosensors and in coatings, plastics, nanowire, nanofiber and textiles and in certain biogenic and bioscience applications.

Key Words: Formula: MnO; CAS Number: 1344-43-0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.0050 - 0.10 µm0.0050 - 0.10 µm
Specific Surface Area 25 - 50 m²/g25 - 50 m²/g
Molecular Weight 70.94 g/mol70.94 g/mol
 
Descriptive Properties
AppearanceGreen Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Rohacell® 200 WF High Heat Grade Polymethacrylimide (PMI) Foam
Chemtotal Manganese Oxide

EJAMER55 / 5538

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.