MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BASF ecovio® FT2341 PLA
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Product Description: ecovio® FT2341 is our new biodegradable film product based on renewable resources. It is basically a compound of our biodegradable, aliphatic aromatic copolyester grades ecoflex® F and ecoflex® FS and a small amount of polylactic acid (PLA). Ecovio® FT2341 has a biobased content of 34%. Due to its outstanding mechanical strength ecovio® FT2341 offers a great down gauging potential needed for very thing film applications like T-shirt, organic waste and fruit & vegetable bags etc. ecovio® FT2341 does not contain slip agents. Ecoflex® slip masterbatches have to be used to tailor the sliding properties required for easy processing of film extrusion and film conversion equipment.

Availability: Europe; North America

Features: Alphatic; Aromatic; Biodegradable; Compostable; Food Contact Acceptable; Good Processability; Good Tear Strength; Good Thermla Stabilty; High Melt Strength; High Strength; Renewable Resource Content; Semi Crystalline

Use: Bags; Blown Film

Agency Ratings: ASTM D6400; DIN EN 13432; EC 1907/2006 (REACH); EU Food Contact; FDA Food Contact

RoSH Compliance: RoSH Compliant

Appearance: Clear/Transparent; Traslucent

Form: Pellets

Processing Method: Blown Film

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.800 g/cc0.0289 lb/in³ISO 60
Density 1.36 - 1.40 g/cc0.0491 - 0.0506 lb/in³ISO 1183
Melt Flow 2.5 - 7.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
2.5 - 7.5 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  21.0 MPa
@Thickness 2.49 mm
3050 psi
@Thickness 0.0980 in
TD, Blown Film; ISO 527-3
 24.0 MPa
@Thickness 2.49 mm
3480 psi
@Thickness 0.0980 in
MD, Blown Film; ISO 527-3
Film Elongation at Break, MD 340 %
@Thickness 2.49 mm
340 %
@Thickness 0.0980 in
Blown Film; ISO 527-3
Film Elongation at Break, TD 610 %
@Thickness 2.49 mm
610 %
@Thickness 0.0980 in
Blown Film; ISO 527-3
Tensile Modulus  0.160 GPa
@Thickness 2.49 mm
23.2 ksi
@Thickness 0.0980 in
TD, Blown Film; ISO 527-3
 0.270 GPa
@Thickness 2.49 mm
39.2 ksi
@Thickness 0.0980 in
MD, Blown Film; ISO 527-3
Elmendorf Tear Strength MD 499 g
@Thickness 2.49 mm
499 g
@Thickness 0.0980 in
Blown Film; ISO 6383-2
Elmendorf Tear Strength TD 304 g
@Thickness 2.49 mm
304 g
@Thickness 0.0980 in
Blown Film; ISO 6383-2
Dart Drop Test 150 g
@Thickness 2.49 mm
0.331 lb
@Thickness 0.0980 in
Blown Film; ASTM D1709A
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 - 120 °C230 - 248 °Fecoflex®
 140 - 155 °C284 - 311 °FPLA
 
Descriptive Properties
Biobased Content0.34ASTM D6866

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2155 / 310848

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.