MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC Dianhydrides & Imides 1000F3SP Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: ULTEM 1000F3SP powder is a RoHS compliant polyetherimide (PEI) powder offering a glass transition temperature (Tg) of 217ºC. This FDA compliant powder is available in a spherical shape with an average particle size (D50) of 15 micron and a maximum particle size (D100) of 75 micron.

Features: Hydrolytic Stability,Chemical Resistance,Miscible with epoxy,High Heat Resistance,Good dimensional stability,Flame Retardant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.780 g/ccISO 1183
Density 1.27 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.700 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.25 %ISO 62-1
Particle Size 15 µmSABIC method
Viscosity 13 cP
@Load 5.00 kg,
Temperature 360 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 109ASTM D785
Ball Indentation Hardness 140 MPaH358/30; ISO 2039-1
Tensile Strength, Yield 105 MPa50 mm/min; ISO 527
Elongation at Break 60 %50 mm/min; ISO 527
Elongation at Yield 6.0 %50 mm/min; ISO 527
Tensile Modulus 3200 MPa1 mm/min; ISO 527
Flexural Strength 160 MPayield, 2 mm/min; ISO 178
Flexural Modulus 3300 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
Gardner Impact 36.0 JASTM D3029
Taber Abrasion, mg/1000 Cycles 10CS-17, 1 kg; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 16.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 33.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.00050
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0025
@Frequency 2.45e+9 Hz
IEC 60250
 0.0060
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Thermal Conductivity 0.240 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 200 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 190 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 211 °CRate B/50; ISO 306
Oxygen Index 47 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 400 °C
Zone 2 340 - 400 °C
Zone 3 345 - 400 °C
Melt Temperature 350 - 400 °CInjection Molding
Mold Temperature 135 - 165 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80001 / 287948

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.