MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller HMC-7RC Sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: HMC-7RC is a hot-applied butyl rubber based adhesive/sealant that bonds to various substrates and creates a permanent seal against moisture, dust, and air intrusion.

Features and Benefits:

  • Has excellent adhesion to glass, EPDM, PVC
  • Has excellent adhesion to painted metal substrates
  • Extremely resistant to both interior and exterior environmental conditions
  • Sag resistance at high temperature
  • Excellent adhesion to automotive paint systems
  • Excellent adhesion to polyethylene film
  • Low temperature flexibility at -29°C (-20°F)
  • Resistant to environmental exposure

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D71
Solids Content 100 %
Ash 24 %FLTM-150-10
Storage Temperature 4.00 - 43.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 0.150 MPaMS-CD641
Penetration 95[dmm], Cone
Peel Strength 11.42 pli9985934
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -40.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Cold SlamPass 10 slams-29°C, GM9773P
ColorBlack
ConsistencyHot Melt
Force to Compress1.1 N/mmASTM C972, 50%, 5 mm diameter bead

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL128 / 316919

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.