Product Description: Celanex 3126 is a non-exuding flame retarded, 10% fiberglass reinforced PBT which has an excellent balance of mechanical properties and processability. It is well suited for electrical connector applications where its UL approved 50% regrind use capability allows maximum use of purchased product. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Filler/Reinforcement: Glass Fiber Additive: Flame Retardant; Impact Modifier; Mold Release Features: Flame Retardant; Impact Modified; Good Heat Resistance Forms: Pellets Processing Method: Injection Molding Information provided by Celanese |